Alloy Digest (1964) 13 (8): Mo-5.
Published: 01 August 1964
... TZM is a molybdenum-base alloy having good formability and good high temperature properties. It is recommended for structural parts operating at very high temperature levels, as well as for tools such as extrusion dies and die casting cores. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2020) 69 (12): Mo-20.
Published: 01 December 2020
... Wieland Duro TZM is a molybdenum-titanium-zirconium-carbon alloy produced from pressed-and-sintered billets. Compared to unalloyed molybdenum, it exhibits higher recrystallization temperature and enhanced high-temperature strength and creep strength. Wieland Duro TZM is typically used between 700...
Journal Articles
Alloy Digest (1967) 16 (2): Mo-8.
Published: 01 February 1967
... arc-cast TZM, which has the same composition. Suggested uses are dies for extrusion, hot pressing, and die casting and for a wide structural components that operate at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...