Alloy Digest (1988) 37 (7): CI-55.
Published: 01 July 1988
... TYPE CR MEEHANITE is an austenitic material especially designed to meet a wide variety of corrosion, wear and heat applications. Like other Meehanite materials it is produced under closely controlled procedures which result in desirable graphite form and distribution. This datasheet provides...
Journal Articles
Alloy Digest (1988) 37 (10): CI-56.
Published: 01 October 1988
... TYPE CRS MEEHANITE is a group of austenitic cast irons with graphite in nodular form. They provide much higher strength than Type CR Meehanites and have excellent resistance to corrosion, wear and heat. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1957) 6 (6): CI-19.
Published: 01 June 1957
... Constants: carbon (total) over 3.0 Specific gravity 7.38 SiiiCOll over 1.0 Thermal conductivity, BTU/hr/ft*/in/°F. 360 other elements cu; cr, MO (50450 F.) Iron Remainder Thermal coef. expansion, in/in/V. 0.00000728 ( 100-lOOO°F.) Modulus of elasticity, psi 2 1,000,000 Modulus of rupture, psi 76,000 Table 1...
Journal Articles
Alloy Digest (1961) 10 (3): CI-29.
Published: 01 March 1961
.... Composition: Carbon Silicon Other elements Iron 3.55 max. 1.90 min. Cu./Cr./Ma. Remainder Physical Constants: Specific gravity 7.16 Thermal conductivity, Btu/hr/ft2/io/OF (50-4500F) 298 Thermal coef. expansion/OF I lo-6 (lOO-10000F) 6.66 Modulus of elasticity, psi I 106 10 Modulus of rupture, psi x 103 61...