Alloy Digest (1995) 44 (3): SS-587.
Published: 01 March 1995
... TYPE 316L-SCQ stainless steel is a cleaner version of AISI Type 316L. The clean microstructure, a reduction in the frequency and severity of non-metallic inclusions, allows a better electroplated surface. The unique applications considered for this microstructurally clean alloy include...
Journal Articles
Alloy Digest (1995) 44 (1): SS-579.
Published: 01 January 1995
...- ered for a wide range of applications which require slightly less corrosion resistance than Type 316L stain- less and does not require electropolishing. The mechanical properties and corrosion resistance of Type 304 SCQ stainless arc identical to those of air- melted Type 304 stainless. The difference...