Alloy Digest (1975) 24 (10): Co-73.
Published: 01 October 1975
... TRIBALOY T-800 consists of a hard, intermetallic phase in a softer, cobalt-base alloy matrix. It can be cast or hardfaced. As alloy powder it can be plasma sprayed or blended with other powders for P/M (Powder Metallurgy) processing. It has excellent resistance to crevice corrosion and it is less...
Journal Articles
Alloy Digest (1996) 45 (9): Co-99.
Published: 01 September 1996
... Tribaloy alloy T-800 was derived from an alloy family developed by DuPont. Excessive amounts of molybdenum and silicon included the formation during solidification of a hard and corrosion-resistant intermetallic coumpound, known as Laves phase. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1996) 45 (10): Co-100.
Published: 01 October 1996
... crack resistance and a lower preheat temperature compared with Tribaloy T-800 (Alloy Digest Co-99, September 1996). This datasheet provides information on composition, microstructure, and hardness. It also includes information on corrosion and wear resistance. Filing Code: CO-100. Producer or source...
Journal Articles
Alloy Digest (2006) 55 (10): Co-114.
Published: 01 October 2006
... castability chemical composition corrosion-resistant alloys fracture toughness hardness joinability oxidation resistance powder metal products shear strength tensile properties TRIBALOY T-400C wear resistance Chemical Composition, wt (Nominal, major elements) T-400 T-400C T-800 Chromium 7.5 14.0...
Journal Articles
Alloy Digest (2006) 55 (8): Co-113.
Published: 01 August 2006
... has better cracking resistance than T-400 or T-800. It is similar to Stellite 12. Fig. 2 Charpy impact test results (unnotched) Fig. 3 High-temperature wear resistance (Plint test). Test method: cylin- der on nitrided 310 stainless steel flat. Cylinder specimen investment cast. Flat specimen nitrided...