Skip Nav Destination
Close Modal
Search Results for
TOUGHMET 3
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-3 of 3 Search Results for
TOUGHMET 3
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (7): Cu-670.
Published: 01 July 2001
... ToughMet 3 is a Cu-15Ni-8Sn alloy. ToughMet is a line of spinoidal alloys for bearings capable of performing with a variety of shafting materials and lubricants. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Abstract
View article
PDF
ToughMet 3 is a Cu-15Ni-8Sn alloy. ToughMet is a line of spinoidal alloys for bearings capable of performing with a variety of shafting materials and lubricants. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion and wear resistance as well as machining. Filing Code: CU-670. Producer or source: Brush Wellman Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (5): Cu-724.
Published: 01 May 2013
... ToughMet 2 is a high performance, wrought, heat treatable, lead-free strip Cu-Ni alloy that imparts superior mechanical performance and high thermal stability to plain bearing applications. Parts are easily formed and they can be machined either before or after heat treatment. ToughMet alloys...
Abstract
View article
PDF
ToughMet 2 is a high performance, wrought, heat treatable, lead-free strip Cu-Ni alloy that imparts superior mechanical performance and high thermal stability to plain bearing applications. Parts are easily formed and they can be machined either before or after heat treatment. ToughMet alloys are a line of spinodal hardened Cu-Ni anti-galling alloys for bearings capable of performing with a variety of shafting materials and lubricants. The alloys combine a high lubricity with wear resistance in these severe loading conditions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming and machining. Filing Code: Cu-724. Producer or source: Materion Brush Performance Alloys. Originally published September 2004, revised May 2013.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (6): Cu-819.
Published: 01 June 2013
... 2. ToughMet and EquaCast are trademarks of Materion Brush Performance Alloys. Table 1 Mechanical properties typical minimum values Temper 0.2% offset yield strength, MPa (ksi) Ultimate tensile strength, MPa (ksi) Elongation, % Hardness, HRC T2 CX90 621 (90) 724 (105) 3 27 Table 2 Tolerances Tube...
Abstract
View article
PDF
ToughMet 2 CX is a Cu-9Ni-6Sn alloy that combines low coefficient of friction with wear resistance. ToughMet alloys are a line of spinodal hardened Cu-Ni antigalling alloys for bearings capable of performing with a variety of shafting materials and lubricants. The alloys combine a high lubricity with wear resistance in these severe loading conditions. ToughMet 2CX in the cast and spinodally hardened (CX) condition exhibits tensile strength in excess of 724 MPa (105 ksi) and hardness exceeding HRC 27 with excellent machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming. Filing Code: Cu-819. Producer or source: Materion Brush Performance Alloys.