Alloy Digest (1962) 11 (1): SA-124.
Published: 01 January 1962
... TORMANC SPECIAL is a low-carbon manganese-nickel-molybdenum steel for locomotive parts, railway and general engineering purposes. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture...