... TOPHET Alloy C has excellent heat resistance to 1850 F (1010 C) and is highly suited for domestic appliance heating elements. Because of its ability to withstand high overloads it is used in heavy-duty rheostats and controls. This Digest supercedes Filing Code Ni-106 of 10/65. This datasheet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (10): Ni-106.
Published: 01 October 1965
... Tophet-C is a nickel-base alloy recommended for electrical appliances and other devices whose operating temperatures do not exceed 1850 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (12): Ni-389.
Published: 01 December 1990
... TOPHET Alloy A has long been used in resistance heating elements serviceable to 2150 F(1175 C). Resistance to chemical corrosion and to carburizing atmospheres broaden the alloy's range of applications. This Digest supercedes Filing Code Ni-39 of 2/58. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (7): Ni-135.
Published: 01 July 1968
... easily be accomplished by lapping rhe two ends to be welded and welding along the edge of the strip. General Characteri sties: Tophet 30 is a nickel-chromium heat resistant alloy developed IO have superior oxidation resistance up to 1260°C (23O(PF) in air or generated exorhermic acmos- pheres, high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (1): Fe-30.
Published: 01 January 1967
... properties, strength and ductility are inherent in the welded joints. Specificotion Equivalents: ASThl B-344 QQ R-175 Compositicm C General Characteristics: Tophet-D is an iron-base alloy having high electrical resistance aodgood oxidation resistance. It is recommended for resistors and rheostats operating...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (2): Ni-39.
Published: 01 February 1958
... TOPHET A is a 80Ni-20Cr alloy recommended for high temperature service. It is recommended for temperatures up to 2100 F. It is also very widely used in chemical applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (2): Ni-162.
Published: 01 February 1971
... that open heating elements of TOPHET H will have a life expactancy approaching those made of 80 nickel-20 chromium TOPHET A alloys. Life expectancy would be greater than for elements made of the 60 nickel-16 chromium TOPHET C alloys. Life tests in sheathed MgO insulated elements indicate life expectancy...