Alloy Digest (1984) 33 (12): TS-433.
Published: 01 December 1984
... TNW is a high-speed steel. It has an optimum alloy composition that combines the good toughness characteristics of a high-molybdenum steel and the excellent abrasion resistance provided by a 2% vanadium content. TNW is a popular choice for twist drills, taps, reamers, router bits, end mills and...