Alloy Digest (2007) 56 (9): TS-655.
Published: 01 September 2007
... The carbon content in TLS S1, about 0.5%, produces a combination of high strength and high toughness with medium wear resistance. Chisels and rivet sets are typical applications. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture...