1-20 of 20 Search Results for

TIMETAL 8-1-1

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (3): Ti-152.
Published: 01 March 2014
... Timetal 8-1-1 is a near alpha alloy with excellent creep resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on forming. Filing Code: Ti-152. Producer or source: Timet. Producer or Source...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (8): Ti-141.
Published: 01 August 2007
... 675 98 262 38 (a) Annealed at 705 °C (1300 °F) for 1 h, air cooled. (b) STA = 885 °C (1630 °F) for 1 h, air cooled, plus 595 °C (1100 °F) for 8 h, air cooled. (c) STOA = 885 °C (1630 °F) for 1 h, air cooled, plus 705 °C (1300 °F) for 1 h, air cooled Fig. 2 Creep comparison (0.2%) between Timetal 6-2-4...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (11): Ti-101.
Published: 01 November 1992
... Weldmult 180 145 8 QOQ F. 8 hrs.) Table 4 - COLD FORMABIIXI Y COMPARISON TIMETAL@ 15-3 Ti-6AL-4V Bend 2.5t 4.5t Springhack lSO 16O Bead 511 - Driw (Cup) 46% - Joggle L/d 2 6 d/t 5 3 Flange Stretch 209b+ - Flange Shrink 1% - StretchWrap 15% 3.5% Heat Treatment: Forms Avallable: Solution anneal at 145OOF...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (12): Ti-144.
Published: 01 December 2007
..., plus heating at 475 °C (887 °F) 8 h, and air cooling. Specification Equivalents: UNS R56260 MIL T-9047 G AMS 4981 Fig. 2 Creep properties; stress for 0.1% total plastic strain in 100 h Fig. 1 Effect of temperature on tensile properties General Characteristics: Timetal 230, a binary alloy containing 2.5...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (2): Ti-104.
Published: 01 February 1993
...@ 1100 Filing Code: Titanium Alloy II-104 FEBRUARY 1993 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS rcloyrkEu- -by:A#oyDipsLInc/201%77-S161 -,a Z~C~W~SO~~D,NJ.O~USOIU.SA TIMETAL 1100 (I-1 100, a hbh strength, high temperature alloy) TIMETALe 1100, a near alpha alloy. was developed for elevated...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (1): Ti-103.
Published: 01 January 1993
... 0.165 1755-1770 16-17 PROPERTlES Table 1 - MINIMUM MECHANICAL PROPERTIES* STA Plate and Forgings to 3-inches Thick Ultimate Tensile Strength ksi, min 150 02% Yield Strength ksi, min 135 Fracture Toughness ksiGbin 70 Elongation 8 in 2-in, min 6 Reduction of Area 8, min 12 Heat Treatments: The best...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (6): Ti-140.
Published: 01 June 2007
...: Condition Treatment, generalized Stress relief anneal 482 649 °C (900 1200 °F) 1 4 h, air cool Mill anneal 704 843 °C (1300 1550 °F), air cool Solution treatment 15 30 °C (25 50 °F) below beta transus, 1 h water quench Aging 538 593 °C (1000 1100 °F) 8 h, air cool Table 2 Creep and Post-Creep Tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (11): Ti-143.
Published: 01 November 2007
... 1275 °F) 2 8 h, air cool. (e) Only for material with thickness 0.187 to <1.75 in. Product Forms Available: This alloy is available in most common product forms including billet, bar, wire, plate, and sheet. Applications: Timetal 6-4 alloy and its variants has been used in air frames, jet engine...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (9): Ti-114.
Published: 01 September 1998
... pressure vessels shear strength tensile properties TIMETAL 3-2.5 TIMETAL 3-2.5 .05Pd weldability workability thermal properties UNS R56320 R56322 I _ - - 7 and Filing Code: li-114 m Titanium I TIMETAL 3-2.5 -1-m-1-1 m a a - mm- I I a 1 TIMETAL 3-2.5.05Pd 1 wa Septetmber 1998 -DIGEST...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (2): Ti-126.
Published: 01 February 2002
... with creep resistance. TIMETAL is a registered trademark of TIMET. Table 1 Typical Mechanical Properties Test temperature Yield strength, 0.2% Tensile strength Elongation Reduction °C °F MPa ksi MPa ksi in 5D, % in area, % Air cooled and aged 20 68 880 127 1030 149 8 30 100 212 829 120 954 138 18 47 200 392...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (6): Ti-156.
Published: 01 June 2014
... in ASTM seawater at (pH 4) at 90 °C (194 °F) or 150 °C (302 °F) for 30 days. Timetal is a registered trademark of Titanium Metals Corporation. Table 1 Creep properties at 427 °C (800 °F) Stress, MPa (ksi) Creep rate % at 50 h Creep rate, mm/mm/h (in./in./h) 69 (10) 0.029 0.0102 (0.0004) 138 (20) 0.108...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (3): Ti-176.
Published: 01 March 2021
... Physical Properties Unit Mechanical Properties (1635) See Tables 1 and 2. Property °C Beta transus (°F) Hot Formability The compressive flow stress values of Timetal 407, Ti-6Al-4V, and Ti-3Al-2.5V are given in Table 3. Table 1 Mechanical properties(a)(b) at room temperature Cooling rate(c) 0.2% proof...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (7): Ti-116.
Published: 01 July 2001
... °F) for 2 h and oil quench. For solutions less than 15 mm (0.6 in air cooling is rec- ommended. Age at 700 °C (1292 °F) for 2 h and air cool. TIMETAL 834 Filing Code: Ti-116 Titanium July 2001 Table 1 Typical Elevated-Temperature Properties Test temperature Yield stregth, 0.2% Tensile strength...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (10): Ti-142.
Published: 01 October 2007
.... Material should be fully heat treated prior to welding and also given a suitable post weld treatment (for example 4-8 h at 550 °C, 1022 °F). The weld zone of material treated in this way will have similar structure and properties to the parent metal. General Characteristics: Timetal 685, a near-alpha alloy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (10): Ti-80.
Published: 01 October 1992
... TIMETAL 10-2-3 is a high fracture toughness titanium-base alloy. It is metallurgically near-beta and is capable of attaining a wide variety of strength levels, depending uopn the selection of heat treatment. Major advantages of this alloy are: (1) Its excellent forgeability, (2) Its high toughness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (10): Ti-105.
Published: 01 October 1998
... Properties: Modulus of elasticity, in tension, 24 C (75 OF), GPa ( IO6 psi) Solution treated 72-85 (10.5-12) Aged 538 C (1000 F) for 8 h 103-110 (15-16) Overaged 96103 (14-15) see also Tables 1-3. Table 1 Typical Room-Temperature Tensile Proper- ties for Strip and Sheet to 0.1875 in. Thick Direction...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (5): Ti-154.
Published: 01 May 2014
... mechanical properties are shown in Tables 1 5. Heat Treatment: Heat treatment Temperature, °C (°F) Solution treat and age (STA) 800 (1475) 4 h, water quench 635 (1175) 8 h, air cool Stress relieve (before finish machining) 550 (1020) 4 h, air cool General Characteristics: Timetal 17 is a high-strength deep...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (7): Ti-180.
Published: 01 July 2021
... excellent cold formability. In the aged condition, the alloy has high strength. It is acceptable for use up to 230 °C (550 °F). Chemical Composition Composition, wt%(a) Mechanical Properties 14.0 16.0 See Tables 1, 2, and 3. Element 2.5 3.5 Vanadium 2.5 3.5 Corrosion Resistance Chromium 2.5 3.5 Tin 0.12...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (9): Ti-66.
Published: 01 September 1992
...-6Al-4V SHEET (Thicknesses up to 0.187 in) Tensile Yield Strength Elongation StTength (0.2% Offset) (2 in.) Condition psi psi % Annealed 144000 136000 14 Solution treated 152000 132000 12 44 168000 :54000 8 Fig. 1 - Effects of temperature on the cryogenic behavior of TibAI-4V ELI sheet. Fig. 2 - Effect...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (5): Ti-166.
Published: 01 May 2020
... conductivity W/(m K) (Btu/(h·ft·°F)) 17.3 (10) Magnetic permeability Nonmagnetic Typical values. (a) At 0 316 °C (32 600 °F) Mechanical Properties See Tables 1 and 2. Corrosion Resistance The general corrosion behavior of ATI 3-2.5 is similar to that of unalloyed commercially pure titanium. The nature...