Alloy Digest (1992) 41 (7): TS-511.
Published: 01 July 1992
... THYROTHERM 2799 is a maraging tool steel with extremely low heat treat distortion and high resistance to thermal shock and excellent weldability. The alloy also possesses resistance to heat checking a high work temperatures. This datasheet provides information on composition, physical properties...