Alloy Digest (1992) 41 (8): TS-512.
Published: 01 August 1992
... THYRAPID 3341 is similar to AISI M2, but adds sulfur. It is general purpose high-speed tool steel with good toughness, red hardness, and excellent machinability. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1998) 47 (2): TS-560.
Published: 01 February 1998
..., cutting tools, broaches, reamers, countersinks, chaser& segments for circular saws, shaping tools. and woodworking tools. Thyrapid is a trademark of Thyssen Specialty Steels, Inc. Chemical Composition, wt (N-1 Carbon 0.90 Chromium 4.1 Molybdenum 5.0 Vanadium 1.9 tigsten 6.4 A similar steel, Thyrapid 3341...