Alloy Digest (2012) 61 (11): CS-173.
Published: 01 November 2012
... The high strength of Tenform XF450, a hot-rolled high-strength low-alloy steel, allows the user to increase the strength of the finished component or to reduce the thickness. Construction and the automotive industries offer uses. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2007) 56 (1): CS-148.
Published: 01 January 2007
... The high strength of Tenform XF450, a hot-rolled high-strength low-alloy steel, allows the user to increase the strength of a finished component or to reduce the thickness. The steel is used in the construction and the automotive industries. This datasheet provides information on composition...