Skip Nav Destination
Close Modal
Search Results for
TENFORM XF350
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
TENFORM XF350
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (12): CS-147.
Published: 01 December 2006
... The high strength of Tenform XF350, a hot-rolled high-strength low-alloy (HSLA) steel, allows the user to increase the strength of the finished component or to reduce the thickness. The material finds use in the construction and the automotive industries. This datasheet provides information...
Abstract
View article
PDF
The high strength of Tenform XF350, a hot-rolled high-strength low-alloy (HSLA) steel, allows the user to increase the strength of the finished component or to reduce the thickness. The material finds use in the construction and the automotive industries. This datasheet provides information on composition, physical properties, and tensile properties as well as fatigue. It also includes information on forming. Filing Code: CS-147. Producer or source: Hille & Mueller, USA Inc.