Alloy Digest (1978) 27 (1): Ni-253.
Published: 01 January 1978
... TECHALLOY Alloy 625 is a nonmagnetic nickel-base alloy with excellent resistance to corrosion and oxidation. It has outstanding strength and toughness from cryogenic temperatures to 2000 F. It also has exceptionally high fatigue strength and is resistant to chloride-ion stress-corrosion cracking...