... TECHALLOY 294 is a copper-nickel alloy with constant electrical resistance over a wide range of temperatures. It is used widely in rheostats and controls where the maximum operating temperature does not exceed 1000 F. Its low temperature coefficient of electrical resistance and its stability make...
Journal Articles
Alloy Digest (1979) 28 (12): Fe-60.
Published: 01 December 1979
... TECHALLOY GLASSEAL 29-17 is an iron-nickel-cobalt alloy with a thermal expansion rate that is unlike most metals and closely matches the thermal expansion characteristics of borosilicate glass, PYREX glass, and other similar low-expansion materials. It assures precisely controlled expansion...