Alloy Digest (1978) 27 (3): SS-348.
Published: 01 March 1978
... TECH-TRONIC 32 stainless steel is essentially a low-nickel chromium-manganese austenitic iron-base alloy. In the annealed condition it provides about twice the yield strength of AISI Type 304 stainless steel and almost the same resistance to corrosion. It also offers improved wear and galling...