Journal Articles
Alloy Digest (1982) 31 (4): Ta-5.
Published: 01 April 1982
... TANTALOY 63 Metal is a tantalum-base alloy containing typically 2.5% tungsten and 0.15% columbium. It is melted in an electron-beam furance. Its strength is considerably greater than that of unalloyed tantalum. For a wide range of chemicals at elevated temperatures, its corrosion resistance...