Alloy Digest (1990) 39 (1): P-15.
Published: 01 January 1990
... TAXTIX 123 and TACTIX 138 resins cured with TACTIX H31 and TAXTIX H41 hardeners are specifically designed to maximum performance properties most critical to advanced composites. This datasheet provides information on composition, physical properties, tensile properties, and compressive strength...
Journal Articles
Alloy Digest (1991) 40 (5): P-26.
Published: 01 May 1991
... strength, ksi Tensile modulus, ksi Elongation, % Flexural strength, ksi Flexural modulus, ksi Glass transition temperature, C Moisture absorbance (200 hour water boil), wt % TACTIX 556 10.5 380 3.7 19.7 450 223 TACTIX 556+ 10% Tactix 123 10.8 410 3.7 19.0 460 230 TACTIX 556+ 10% D.EN.t 431 9.6 460 2.7...