Alloy Digest (1959) 8 (5): Ti-19.
Published: 01 May 1959
... T1-155A is a titanium alloy having guaranteed heat treat capability up to 175,000 psi tensile strength for bark stock and 180,000 psi for forging stock. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength...