Alloy Digest (2002) 51 (12): Cu-695.
Published: 01 December 2002
... Swissmetal alloy SM931R is an alloy designed for hot working and contains a duplex alpha plus beta microstructure. The alloy has also been called DORECO. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength. It...