Alloy Digest (2002) 51 (6): Cu-683.
Published: 01 June 2002
... Swissmetal alloy SM158N (Boillat 61B) is a free-machining brass with both machinability and cold workability. The alloy has been called heavy-leaded brass, clock brass, and engraver’s brass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...