Alloy Digest (2001) 50 (6): Cu-668.
Published: 01 June 2001
... Swissmetal SM453C is a free-machining copper alloy with high electrical conductivity. It is recommended for male contacts in electrical and electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...