1-9 of 9 Search Results for

Supra 50

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2017) 66 (8): Fe-167.
Published: 01 August 2017
... SUPRA 50 is a soft magnetic alloy with close to 50% nickel. It typically runs 47.5 Ni; 0.5 Mn, 0.1 Si; and 0.005 C This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: Fe...
Journal Articles
Alloy Digest (2012) 61 (4): Fe-159.
Published: 01 April 2012
... Supra 36 is a Fe-Ni alloy with 36% nickel content that exhibits the highest electrical resistivity in the Fe-Ni system. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, and machining...
Journal Articles
Alloy Digest (2010) 59 (8): TS-690.
Published: 01 August 2010
... Thermodur 2367 Supra is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength and thermal conductivity) are required to resist thermal fatigue and tempering. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2007) 56 (6): TS-651.
Published: 01 June 2007
... Thyrodur 2767/2767 Supra is a cold-work tool steel with high hardenability for punching tools. Thyrodur 2767 Supra is the electroslag remelted version. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating. Filing Code...
Journal Articles
Alloy Digest (2015) 64 (9): SS-1224.
Published: 01 September 2015
... Outokumpu Supra 316LN/4429 is a grade that can be used in applications with increased demand for corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as...
Journal Articles
Alloy Digest (1993) 42 (1): TS-515.
Published: 01 January 1993
... Thyroplast 2083 and 2083 SUPRA ESR steels are double tempered after a vacuum hardening treatment to develop a high hardness with excellent toughness. Vacuum degassing and ESR remelting assure superior cleanliness. High strength to 300 KSI is attainable. This datasheet provides information on...
Journal Articles
Alloy Digest (1994) 43 (9): SS-572.
Published: 01 September 1994
... THYROPLAST 2083 SUPRA ESR is an electroslag remelted (ESR) stainless tool steel (modified AISI 420) with cleanliness for polishing and good toughness and erosion resistance. This datasheet provides information on composition and physical properties. It also includes information on heat treating...
Journal Articles
Alloy Digest (1994) 43 (6): TS-527.
Published: 01 June 1994
... SUPRA ESR has the capability of achieving Rc 44- 50 for die casting with notched chatpy impact values in excess of 13 Joules, typical in excess of 18 Joules. It is heat treated to Rc 52-54 for plastic molding applications. When employed as a plastic mold, lhyrothetm 2344 SUPRA ESR has cleanliness and...
Journal Articles
Alloy Digest (1993) 42 (9): SA-468.
Published: 01 September 1993
... (S) in mm in/tooth mm/tooth 0.08 min 2 min 0.008 min 0.20 min 0.08 max 2max 0.008 max 0.20 max Tool Type P.30-P.40 H.S.S. P. lo-P.20 H.S.S. Cutting Speed (V) fpm m/min 230-330 70-100 50-100 15-30 295-380 90-115 65-115 20-35 TYPICAL DRILLING PARXvIETERS FOR THYSSEN 4140 HOLDER Hole Diameter Depth of...