Journal Articles
Alloy Digest (2004) 53 (5): SS-903.
Published: 01 May 2004
... Supermet 2205 is a manual metal arc (MMA) electrode with enhanced chromium, molybdenum, and nitrogen levels. It is used for welding standard 22% Cr duplex austenitic/ferritic stainless steels. This datasheet provides information on composition, microstructure, hardness, and tensile properties as...
Journal Articles
Alloy Digest (2007) 56 (8): SS-995.
Published: 01 August 2007
..., 52N, 52N+ (CLI); Ferrinox 255 (Advanced Metals) Product Forms Available: Supermet 2205 is available in the size, weight, and pieces shown below: Diameter, mm Length, mm Weight, kg/carton Pieces/carton 2.5 300 12.0 630 3.2 350 13.2 354 4.0 350 13.8 255 5.0 450 18.6 165 Applications: Supermet 2506 Cu...