Skip Nav Destination
Close Modal
Search Results for
Sumitomo SM2242-125
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Sumitomo SM2242-125
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2017) 66 (8): Ni-734.
Published: 01 August 2017
... Sumitomo SM2242-125 is a high strength austenitic alloy for use in oil country tubular goods as a material suitable for severe sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion...
Abstract
View article
PDF
Sumitomo SM2242-125 is a high strength austenitic alloy for use in oil country tubular goods as a material suitable for severe sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Ni-734. Producer or source: Nippon Steel and Sumitomo Metal Corporation.