1-1 of 1 Search Results for

Sumitomo SM110XS

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2015) 64 (5): CS-188.
Published: 01 May 2015
... Sumitomo SM110XS is a low-alloy, high-strength carbon steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance...