Alloy Digest (2018) 67 (11): sa-829.
Published: 01 November 2018
... Strenx 960 is a structural steel that guarantees a minimum yield strength of up to 960 MPa (139 ksi) depending on thickness. Strenx 960 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures where low...
Journal Articles
Alloy Digest (2018) 67 (12): sa-832.
Published: 01 December 2018
... Strenx 960 PLUS is a high-strength structured strip steel with minimum yield strength of 960 MPa (139 ksi). It provides excellent thickness, accuracy, and surface quality in relation to the strength. This datasheet provides information on composition, physical properties, tensile properties, and...
Journal Articles
Alloy Digest (2016) 65 (11): SA-772.
Published: 01 November 2016
... Strenx 960MC is a hot-rolled structural steel made for cold forming, with minimum yield strength of 960 MPa (139 ksi) for stronger and lighter structures. This alloy meets or exceeds the requirements of S960MC in EN 10149-2. This datasheet provides information on composition, physical properties...