1-6 of 6 Search Results for

Strenx 900

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2018) 67 (9): SA-821.
Published: 01 September 2018
... Strenx 900 is a structural steel that guarantees a minimum yield strength of up to 900 MPa (131 ksi) depending on thickness. Strenx 900 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures, where low...
Journal Articles
Alloy Digest (2018) 67 (10): SA-826.
Published: 01 October 2018
... Strenx 900 Plus is a structural steel with a minimum yield strength of 900 MPa (131 ksi). Strenx 900 Plus provides a good combination of strength and toughness together with good workshop properties. Typical applications include load-bearing structures, where low weight is needed. This datasheet...
Journal Articles
Alloy Digest (2017) 66 (7): SA-792.
Published: 01 July 2017
... Strenx Section 900 is a cold-formed steel section made of hot-rolled, high-strength steel with a minimum yield strength of 900 MPa (131 ksi). Its high strength combined with naturally stiff form enables construction of stronger and lighter structures. The common shape is a U-bend channel...
Journal Articles
Alloy Digest (2016) 65 (9): SA-766.
Published: 01 September 2016
... Strenx 900MC (minimum yield strength of 900 MPa, or 130 ksi) is one alloy in an extensive portfolio of high-strength, high performance structural steels. Strenx 900MC has good welding, cold forming, and cutting performance. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2018) 67 (11): sa-829.
Published: 01 November 2018
... 1150 (142 167) 53.1 100 mm (2.09 3.94 in.) thickness 900 1100 (131 160) Elongation, A5, min, % 4.0 53.0 mm (0.16 2.09 in.) thickness 12 53.1 100 mm (2.09 3.94 in.) thickness 10 DOI: 10.31399/asm.ad.sa0829 Fabricability Welding, Bending, and Machining. Strenx 960 has good welding, cold forming...
Journal Articles
Alloy Digest (2017) 66 (2): SA-779.
Published: 01 February 2017
... (3.94 6.30) 650 (94) 710 900 (103 131) 14 (a) For transverse test pieces according to EN 10025 DOI: 10.31399/asm.ad.sa0779 Bending. Tolerances according to Strenx Bending Guarantee Class A. Specification Equivalents: EN 10025-6 EN 10029 EN 10163-2 General Characteristics: The alloy is a high-strength...