Alloy Digest (2018) 67 (8): SA-819.
Published: 01 August 2018
... Strenx 700 CR is a cold-rolled structural steel with a minimum yield strength of 700 MPa (102 ksi) used to produce stronger and lighter structures. Strenx 700 CR has good cold forming, welding, and cutting performance. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2017) 66 (2): SA-779.
Published: 01 February 2017
... Strenx 700 is a high-strength structural steel with a minimum yield strength of 650–700 MPa (94–102 ksi) depending on thickness. Strenx 700 meets the requirements of EN 10 025-6 for the S690 grade and thicknesses. Typical applications include demanding load-bearing structures. This datasheet...
Journal Articles
Alloy Digest (2018) 67 (4): SA-815.
Published: 01 April 2018
... Strenx 700 OME is a structural steel with a minimum yield strength of 700 MPa (102 ksi) developed for use in demanding load-bearing structures within the offshore and marine industry. Strenx 700 OME exceeds the requirements of S690QL, EN 10 025-6. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2016) 65 (8): SA-763.
Published: 01 August 2016
... Strenx 700MC is a hot-rolled structural steel made for cold forming, with minimum yield strength of 700 MPa (102 ksi) for stronger and lighter structures. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness...
Journal Articles
Alloy Digest (2018) 67 (7): SA-817.
Published: 01 July 2018
... in the name indicates the minimum yield strength in MPa. Strenx is a trademark of SSAB Swedish Steel, Inc. Chemical Composition, wt.% (Typical, maximum) Sum of Nb, V, and Ti = 0.22%, max. The steel is grain refined. CET = C + (Mn+Mo)/10 + (Cr+Cu)/20 + Ni/40 CEV = C + Mn/6 + (Cr+Mo+V)/5 + Cu+Ni/15 Carbon...
Journal Articles
Alloy Digest (2019) 68 (2): SA-838.
Published: 01 February 2019
... to Strenx 700 (Alloy Digest SA-779). Strenx is a trademark of SSAB Swedish Steel, Inc. Chemical Composition, wt.% (Typical, maximum) The steel is grain refined. Carbon equivalent information is given in Table 1. CEV = C + Mn/6 + (Cu+Ni)/15 + (Cr+Mo+V)/5 CET = C + (Mn+Mo)/10 + (Cr+Cu)/20 + Ni/40 Carbon...
Journal Articles
Alloy Digest (2016) 65 (7): SA-759.
Published: 01 July 2016
..., such as those demanding a load-bearing structure. Producer: SSAB Swedish Steel, Inc. Pittsburgh, PA 15225, USA Tel: (412) 269-2100 Fax: (412) 269-2124 In Sweden: SSAB Tunnplat AB Borlange 781 84 Tel: +46-243-700-00 Fax: +46-243-720-00 www.ssab.com ISSN: 002-614X SA-759B SSAB s Strenx guarantees include tight...
Journal Articles
Alloy Digest (2019) 68 (12): SA-859.
Published: 01 December 2019
... Strenx 1100 CR is a cold-rolled structural steel with a minimum yield strength of 1100 MPa (160 ksi) for stronger and lighter structures. This material is available as cut-to-length sheets. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code...
Journal Articles
Alloy Digest (2018) 67 (11): sa-829.
Published: 01 November 2018
..., welding, cutting, grinding, or otherwise working on the product. Strenx 700-960 can be stress relieved by post-weld heat treatment, although this is seldom necessary. Other Strenx and Hardox steels should not use this method for stress relieving, since this may impair the mechanical properties. Welding...
Journal Articles
Alloy Digest (2017) 66 (4): SA-780.
Published: 01 April 2017
... Strenx Section 700 is a cold-formed steel section made of hot-rolled, high-strength steel with a minimum yield strength of 700 MPa (102 ksi). Its high strength combined with naturally stiff form enables construction of stronger and lighter structures. The common shape is a U-bend channel...
Journal Articles
Alloy Digest (2016) 65 (12): SA-773.
Published: 01 December 2016
... Strenx 1100 MC is a high-strength hot-rolled structural steel made for cold forming, with minimum yield strength of 1100 MPa (160 ksi) for stronger and lighter structures. This alloy meets or exceeds the requirements of S1100 MC in EN 10149-2. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2017) 66 (6): SA-788.
Published: 01 June 2017
... in.) = C + Mn/6 + (Cu+Ni)/15 + (Cr+Mo+V)/5 CET = 0.22; 2.5 10 mm (0.1 0.4 in.) = C + (Mn+Mo)/10 + (Cr+Cu)/20 + Ni/40 Physical Constants: (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.280) Copyright © 2017, ASM International®. All rights reserved. STRENX SECTION 650 (Structural Steel) Filing Code: SA-788...
Journal Articles
Alloy Digest (2017) 66 (5): SA-783.
Published: 01 May 2017
... (0.16 0.39 in.) = 0.67 CEV = C+Mn/6 + (Cu+Ni)/15 + (Cr+Mo+V)/5 CET of 1300E and 1330F for 4.0 10.0 mm (0.16 0.39 in.) = 0.43 CET = C + (Mn+Mo)/10 + (Cr+Cu)/20 + Ni/40 Physical Constants: (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.280) Copyright © 2017, ASM International®. All rights reserved. STRENX...
Journal Articles
Alloy Digest (2019) 68 (1): SA-834.
Published: 01 January 2019
... Strenx 1100 is a structural steel that guarantees a minimum yield strength of 1100 MPa (160 ksi). Strenx 1100 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures, where low weight is needed. Despite...
Journal Articles
Alloy Digest (2018) 67 (10): SA-826.
Published: 01 October 2018
... Strenx 900 Plus is a structural steel with a minimum yield strength of 900 MPa (131 ksi). Strenx 900 Plus provides a good combination of strength and toughness together with good workshop properties. Typical applications include load-bearing structures, where low weight is needed. This datasheet...
Journal Articles
Alloy Digest (2016) 65 (6): SA-756.
Published: 01 June 2016
... Steel, Inc. Moon Township, PA 15108, USA Tel: +1-412-203-1620 Fax: +1-412-203-1650 In Sweden: SSAB Tunnplat AB Borlange 781 84 Tel: +46-243-700-00 Fax: +46-243-720-00 www.ssab.com ISSN: 002-614X SA-756B Product Forms Available: Strenx 600 MC comes in coils, slit coils, or cut-to-length sheets. Dimension...
Journal Articles
Alloy Digest (2016) 65 (11): SA-772.
Published: 01 November 2016
... Strenx 960MC is a hot-rolled structural steel made for cold forming, with minimum yield strength of 960 MPa (139 ksi) for stronger and lighter structures. This alloy meets or exceeds the requirements of S960MC in EN 10149-2. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2018) 67 (9): SA-821.
Published: 01 September 2018
... in.) 0.39 80.1 100 mm (3.15 3.94 in.) 0.41 Carbon equivalent information CEV = C + Mn/6 + (Cu+Ni)/15 + (Cr+Mo+V)/5 CET = C+ (Mn+Mo)/10 + (Cr+Cu)/20 + Ni/40 Physical Constants (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.279) Copyright © 2018, ASM International®. All rights reserved. STRENX 900...
Journal Articles
Alloy Digest (2016) 65 (9): SA-766.
Published: 01 September 2016
...-2120 Fax: (412) 269-2124 www.swedishsteel.us In Sweden: SSAB Tunnplat AB Borlange 781 84 Tel: +46-243-700-00 Fax: +46-243-720-00 www.ssab.com ISSN: 002-614X SA-766B General Characteristics: The alloy is a high-strength structural steel at 900 MPa (131 ksi). Strenx 900 MC is a hot-rolled structural...
Journal Articles
Alloy Digest (2018) 67 (12): sa-832.
Published: 01 December 2018
... Strenx 960 PLUS is a high-strength structured strip steel with minimum yield strength of 960 MPa (139 ksi). It provides excellent thickness, accuracy, and surface quality in relation to the strength. This datasheet provides information on composition, physical properties, tensile properties...