Alloy Digest (2016) 65 (7): SA-759.
Published: 01 July 2016
... Strenx 650MC is a high-strength hot-rolled structural steel made for cold forming, with minimum yield strength of 650 MPa (94 ksi) for stronger and lighter structures. This alloy meets or exceeds the requirements of S650MC in EN 10149-2. This datasheet provides information on composition, physical...