Alloy Digest (2019) 68 (2): SA-838.
Published: 01 February 2019
... Strenx 100 is a high-strength, high-performance structural steel with a minimum yield strength of 690 MPa (100 ksi). It meets the requirements of ASTM A514 Grade S. Strenx 100 is a US Customary steel similar to Strenx 700 (Alloy Digest SA-779, February 2017). This datasheet provides information...
Journal Articles
Alloy Digest (2018) 67 (11): sa-829.
Published: 01 November 2018
... 0.70 Boron 0.005 Iron bal CEV 4.1 34.8 mm (0.16 1.37 in.) 0.58 35.1 100 mm (1.38 3.94 in.) 0.38 CET 4.1 34.8 mm (0.16 1.37 in.) 0.67 35.1 100 mm (1.38 3.94 in.) 0.41 Physical Constants (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.279) Copyright © 2018, ASM International®. All rights reserved. STRENX...
Journal Articles
Alloy Digest (2018) 67 (9): SA-821.
Published: 01 September 2018
... in.) 0.39 80.1 100 mm (3.15 3.94 in.) 0.41 Carbon equivalent information CEV = C + Mn/6 + (Cu+Ni)/15 + (Cr+Mo+V)/5 CET = C+ (Mn+Mo)/10 + (Cr+Cu)/20 + Ni/40 Physical Constants (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.279) Copyright © 2018, ASM International®. All rights reserved. STRENX 900...
Journal Articles
Alloy Digest (2018) 67 (4): SA-815.
Published: 01 April 2018
... Strenx 700 OME is a structural steel with a minimum yield strength of 700 MPa (102 ksi) developed for use in demanding load-bearing structures within the offshore and marine industry. Strenx 700 OME exceeds the requirements of S690QL, EN 10 025-6. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2018) 67 (10): SA-826.
Published: 01 October 2018
... of 4 100 mm (0.16 3.94 in while Strenx 900F complies with S890QL1 and is available in the thickness range up to 80 mm (3.15 in Benefits include: High impact toughness, which provides for good resistance to fractures Superior bendability and surface quality Weldability with excellent HAZ strength...
Journal Articles
Alloy Digest (2019) 68 (1): SA-834.
Published: 01 January 2019
... Strenx 1100 is a structural steel that guarantees a minimum yield strength of 1100 MPa (160 ksi). Strenx 1100 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures, where low weight is needed. Despite...
Journal Articles
Alloy Digest (2018) 67 (12): sa-832.
Published: 01 December 2018
... Strenx 960 PLUS is a high-strength structured strip steel with minimum yield strength of 960 MPa (139 ksi). It provides excellent thickness, accuracy, and surface quality in relation to the strength. This datasheet provides information on composition, physical properties, tensile properties...
Journal Articles
Alloy Digest (2019) 68 (11): SA-856.
Published: 01 November 2019
... Strenx™ 1100 Plus is a high-strength, hot-rolled, quenched and tempered, structural steel with a minimum yield strength of 1100 MPa (160 ksi) and very good weld performance. The strength, elongation, and impact toughness of weldments fulfill minimum guarantees of the base metal. This datasheet...