Alloy Digest (2021) 70 (3): Ni-768.
Published: 01 March 2021
... Special Metals Inconel C-276 is a wrought, Ni-Mo-Cr-Fe-W alloy that has excellent corrosion resistance in a wide range of aggressive media. The high molybdenum content makes the alloy especially resistant to pitting and crevice corrosion. The low carbon content minimizes carbide precipitation...
Journal Articles
Alloy Digest (2003) 52 (1): SS-871.
Published: 01 January 2003
... of its corrosion resistance when autogenously welded or when welded with matching com- position filler metal. Overmatching composition welding products with higher molybdenum content are used such as Inconel Filler Metals 622, C-276, and 686CPT, Inconel Welding Electrodes 122 and C-276, and Inco-Weld...
Journal Articles
Alloy Digest (2008) 57 (1): Ni-657.
Published: 01 January 2008
... Werkstoff Nr. 2.4886 BS 2901 NA48 DIN 1736 SG-NiMo16Cr16W EN ISO 18274 SNi6276 (NiCr15Mo16Fe6W4) For manufacture to ASME III (NCA3800, NB2400) and other specification, contact the producer. General Characteristics: This alloy is used for the gas tungsten arc and gas metal arc welding of Inconel alloy C-276...
Journal Articles
Alloy Digest (2005) 54 (12): Ni-629.
Published: 01 December 2005
... Code: Ni-629. Producer or source: Special Metals Corporation. Producer or Source: Special Metals Corporation Copyright © ASM International® 2005 2005 ASM International chemical composition corrosion-resistant alloys elasticity hardness Inconel alloy 050 physical properties tensile...
Journal Articles
Alloy Digest (2019) 68 (8): Ni-754.
Published: 01 August 2019
... requirement of the 9% nickel steels and excellent Charpy impact toughness at 196 °C ( 321 °F). Inco-Weld and Inconel are a Special Metals Welding Products Company trademark. Chemical Composition, wt.% (Type analysis, maximum) Carbon 0.02 Manganese 1.0 Iron 4.0 7.0 Phosphorous 0.04 Sulfur 0.03 Silicon 0.02...
Journal Articles
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
... as well as joining. Filing Code: Ni-624. Producer or source: Special Metals Corporation. Producer or Source: Special Metals Corporation Copyright © ASM International® 2005 2005 ASM International chemical composition corrosion-resistant alloys corrosivity elasticity hardness INCONEL ALLOY...
Journal Articles
Alloy Digest (1992) 41 (10): Ni-414.
Published: 01 October 1992
...= 15Sc Corrosion Resistance: Inconel Filler Metal 622 is an excellent dissimilar metal welding product that offers protection against preferential weld-metal corrosion attack when used for joining mo- lybdenum containing stainless steels as well as the nickel alloys Inconel alloy 622, alloy C-276...
Journal Articles
Alloy Digest (1972) 21 (6): SA-276.
Published: 01 June 1972
... Filing Code: SA-276 Steel-Alloy Or JUNE 1972 DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS Pvblisbd by CRYONIC* 5 Engineering Alloys Digesr, Inc. (Alloy Steel for Low-Temperature Applications) Upper Montclair, New Jersey CRYQNlC 5 is a 5% nickelXt.5m manganesea.25k molybdenum steel designed and specialty...
Journal Articles
Alloy Digest (2015) 64 (10): SS-1229.
Published: 01 October 2015
... and can be welded similar to normal austenitic stainless steel using Inconel 82, Inconel 625, and Hastelloy C-276 welding materials Product Forms Available: This alloy is available in a wide range of plate, sheet, and strip (see Fig. 3). This material requires special consultation for sheet thicknesses...
Journal Articles
Alloy Digest (2008) 57 (1): SS-1006.
Published: 01 January 2008
... temperatures and thus retain good mechanical properties. Inconel is a registered trademark of the Special Metals Group of Companies Table 1 Typical Tensile Properties as Function of Temperature Temperature Yield strength Tensile strength ºC ºF MPa ksi MPa ksi Elongation, % 21 69.8 276 40 587 85 43 225(a) 33...