Alloy Digest (1956) 5 (1): SA-36.
Published: 01 January 1956
... SICROMO-2 is a low-carbon, silicon-chromium-molybdenum steel recommended for those applications at temperatures up to 1200 F. in which a high resistance to oxidation is required. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1953) 2 (2): SA-7.
Published: 01 February 1953
... SICROMO 7M is a low carbon, 7% chromium alloy steel possessing high temperature properties and high resistance to attack by hot petroleum products. It is suggested as a substitute for the 5% chromium type steels for those applications in which a greater resistance is required to corrosion by hot...
Journal Articles
Alloy Digest (1967) 16 (8): SA-215.
Published: 01 August 1967
... changed by long heating under stress ar the temperatures considered.) B. Hot Ductility of More Prolonged Stress-Rupture Specimens Test Time Reduction Temperature Stress for Fracture Elongation of Area OF psi Hours S; in 2 % (Sicromo 9M possesses a temperatures considered.) 1100 16000 2814 31.0 70.1 1200...
Journal Articles
Alloy Digest (1957) 6 (12): SA-64.
Published: 01 December 1957
... considered. C. Hot Ductilitv of More Prolonged Stress-Rupture Specimens. SUIZSS Time for Elongation Reduction psi Fracture, hrs. 70 in 2 of Area, R 18000 1385 52.5 84.1 1100 1200 1300 1500 3500 1200 2068 1920 59.5 78.2 50.7 81.8 Not Fractured Not Fractured 27.5 44.3 Sicromo 3 steel possesses a high degree...
Journal Articles
Alloy Digest (1955) 4 (3): SA-28.
Published: 01 March 1955
..., then air cooled to room temperature and broken). Heating Room Temperature Charpy Value in Foot-Pounds Temperature After 1 Hour at Heat After 1000 Hours at Heat 85 F. 58 - 9OO F. 64 1000 F. ii 76 1100 F. 60 1200 F. 65 74 1300 F. 76 71 1400°F. 1500°F. 2 - - Sicromo 7 steel does not become brittle on long...
Journal Articles
Alloy Digest (1969) 18 (12): SS-232.
Published: 01 December 1969
... SICROMO-5S is a low-carbon, 5% chromium alloy steel recommended for applications in which a high degree of surface stability under oxidizing conditions is required for temperatures up to 1500 F. It is used in air prehealer tubes, recuperater and superheater tubes. This datasheet provides...