... SICROMO-5S is a low-carbon, 5% chromium alloy steel recommended for applications in which a high degree of surface stability under oxidizing conditions is required for temperatures up to 1500 F. It is used in air prehealer tubes, recuperater and superheater tubes. This datasheet provides...