Alloy Digest (1957) 6 (1): Cu-46.
Published: 01 January 1957
... SEYMOUR No. 950 is a 5% tin bronze containing about 0.15% phosphorus. It has high corrosion and fatigue resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion...