Alloy Digest (1964) 13 (8): TS-150.
Published: 01 August 1964
... Seneca Hot Die is a tungsten-chromium-vanadium type hot work steel having good red hardness and abrasion resistance. It is recommended for forging dies, copper extrusion dies, die casting dies, and other hot work tools and dies. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1954) 3 (10): TS-25.
Published: 01 October 1954
... operating temperatures as high as 1000 deg. F for long periods, but it is not recommended for applications subjected to extremely rapid blows. (Water cooling Seneca dies in operation is dangerous and may result in premature checking and cracking). Formerly known as Atlas Hot Die. Forms Available: Billets...