Skip Nav Destination
Close Modal
Search Results for
Schmelzmetall Hovadur CC
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Schmelzmetall Hovadur CC
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (5): Cu-920.
Published: 01 May 2021
...: Schmelzmetall AG Copyright © ASM International® 2021 2021 ASM International Schmelzmetall Hovadur CC chemical composition physical properties elasticity tensile properties corrosion-resistant alloys workability heat treatability machinability joinability UNS C17500 SCHMELZMETALL HOVADUR...
Abstract
View article
PDF
Schmelzmetall Hovadur CCB is a heat-treatable, copper-cobalt-beryllium alloy. In the solution heat treated and artificially aged condition, this alloy combines good mechanical strength and excellent ductility as well as high softening temperature with good thermal and electrical conductivity. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-920. Producer or source: Schmelzmetall AG.