Alloy Digest (2019) 68 (7): SS-1307.
Published: 01 July 2019
... Sanicro 28 is a high alloy for oil country tubular goods with cold work in the alloy for high strength. See Alloy Digest SS-831, September 2001, which covers the use of Sanicro 28 as a superheater material for waste-derived fuel plants. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2001) 50 (9): SS-831.
Published: 01 September 2001
... Sandvik Sanicro 28 composite tube is used in services as superheater material for waste-derived fuel plants. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1984) 33 (3): SS-442.
Published: 01 March 1984
... SANDVIK Sanicro 28 is an all-purpose low-carbon stainless steel alloy for service in highly corrosive environments. It has exceptionally high resistance to various types of corrosive attack and has good weldability. Among its numerous applications are evaporator tubes in the production...
Journal Articles
Alloy Digest (2014) 63 (3): SS-1169.
Published: 01 March 2014
... measurements on Sanicro 28. In Fig. 2, CPT values are presented as a function of pH. Stress Corrosion Cracking. Environmental assisted cracking, especially in the presence of hydrogen sulfide (H2S), is a serious form of corrosion in sour environments. Sanicro 29 possesses very good resistance to conditions...
Journal Articles
Alloy Digest (1992) 41 (4): SS-526.
Published: 01 April 1992
... isocorrosion performance of du- plex SAF 2507 stainless is somewhat better lhan the highly alloyed austenitic SANICRO 28 (27 Cr/31 Ni/ 3.5 MO) and both are superior IO AISI Type 316L (see Fig. 2). In H2S04 at this same corrosion rate. (1 .O% Offset MPa 640 530 485 450 435 425 425 425 (tin) Hardn&s. % Vickea 25...
Journal Articles
Alloy Digest (2004) 53 (7): Ni-622.
Published: 01 July 2004
... 100 338 49.0 68 Table 2 Comparative Corrosion Resistance Corrosion rate, average, mils/yr Media G-35 G-30 Sanicro 28 65% nitric acid, boiling 2.8 3.6 2.3 10% hydrofluoric acid, 52 °C (125 °F) 7.5 22.7 66.2 10% sulfuric acid, 93 °C (200 °F) 0.2 0.2 41.2 50% sulfuric acid, 66 °C (150 °F) 0.1 0.2 11.4 5...
Journal Articles
Alloy Digest (2017) 66 (11): Ni-739.
Published: 01 November 2017
... Sandvik Sanicro 72HP is a corrosion- and oxidation-resistant grade (CRA) available as wire, particularly weld wire. Sanicro 72HP is commonly used as weld wire for joining NiCrFe alloys. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (2018) 67 (9): SS-1293.
Published: 01 September 2018
...) 210 (30.5) 520 (75) 600 (1112) 180 (26) 205 (30) 500 (72.5) 650 (1202) 180 (26) 210 (30.5) 480 (70) 700 (1292) 180 (26) 195 (28) 455 (66) 750 (1382) 180 (26) 195 (28) 410 (59) 800 (1472) 180 (26) 195 (28) 355 (51.5) Table 2 Creep properties of Sandvik Sanicro 25 Temperature, °C (°F) Creep properties...
Journal Articles
Alloy Digest (1965) 14 (12): Ni-108.
Published: 01 December 1965
... Sanicro 71 is a nickel-base alloy having good resistance to stress-corrosion, oxidation and creep at elevated temperatures. It is recommended for nuclear power reactor heat exchanger tubes, aircraft turbojet engines and for equipment in the textile, plastic, and chemical industries. This datasheet...
Journal Articles
Alloy Digest (1996) 45 (8): SA-483.
Published: 01 August 1996
... Sandvik Sanicro 38/4L7 is a composite tube consisting of Sanicro 38, a corrosion-resistant nickel-base alloy on the outside diameter, and carbon steel (A210 GrA-1) for water-wetted service on the inside. The design is placed entirely on the inside tube; however, there is a contribution from both...
Journal Articles
Alloy Digest (1989) 38 (8): SS-267.
Published: 01 August 1989
... (390-570OF). Post weld heat treatment is not necessary where use at high tempera- tures for long times is anticipated. Forotherserviceconditions or wheredesignconsiderationscallforpost-weldthermaltreatment. anneal at 800900°C (1470-1650 F). Sandvilc 29.9, 25.51.25.20 and Sanicro 72 tiller materials...
Journal Articles
Alloy Digest (1997) 46 (11): SS-699.
Published: 01 November 1997
...- mends wire electrodes and rods Sandvik 72. In manual metal-arc welding covered ekcmdes Sandvik Sanicro 72 are recom- mended. For application at temperatures up to 400 C (750 m. welding wire/d Sandvik 19.9.NbSi. 19.9.Nb. 19.9.LSi or 19.9.L and covered electmdes Sandvik 19.9.NbR or 19.9LR are recommended...
Journal Articles
Alloy Digest (2001) 50 (1): SS-812.
Published: 01 January 2001
... is somewhat impaired. For service in this temperature range, the producer recommends the use of Sandvik Sanicro 31HT (see Alloy Digest SS-643), which has better struc- tural stability. Maximum service temperature in air is 1100 °C (2010 °F). Product Forms Available: Seamless tube and pipe are generally...