Alloy Digest (2010) 59 (7): Zr-13.
Published: 01 July 2010
... elasticity joinability machinability physical properties Sandvik zirconium 702 tensile properties workability DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2010, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM...
Journal Articles
Alloy Digest (2003) 52 (10): Zr-11.
Published: 01 October 2003
... advantage. Zirconium has poor resistance to concentrated chloride, wet chlorine, and other oxi- dizing chloride environments. Specification Equivalents: Casting grade 702C is identical in composition and similar in properties to its wrought equivalent UNS R60702, which is grade 702. The casting grade is...