Journal Articles
Alloy Digest (1997) 46 (8): Ti-108.
Published: 01 August 1997
... Sandvik titanium Grade 2 is chemically pure (CP) titanium produced as seamless and SeamFree tubing. The alloy is resistant to a wide variety of chloride media and is used to handle seawater. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1997) 46 (10): Ti-110.
Published: 01 October 1997
... Sandvik Ti-0.3Mo-0.8Ni Grade 12 is used in applications similar to those for unalloyed titanium, but it has better strength and corrosion resistance, particularly in hot brine. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1997) 46 (9): Ti-109.
Published: 01 September 1997
...-3Al-2.5V Grade 9 tensile properties workability thermal properties UNS R56320 1 SANDVIKTi=3A- GRADE9 15 2 septombor 1997 rALs AND ALLOYS u DATA ON WORLD WIDE MEl SANDVIK Ti-3AI-2.W GRADE 9 (Corrosion-Resistant High-Strength Tiinium Alloy) Sandvik li-3AL2.5V Grade 9 titanium-aluminum alloy...
Journal Articles
Alloy Digest (2014) 63 (9): Ti-157.
Published: 01 September 2014
... Sandvik Bioline Ti6Al4V ELI is an alpha-beta titanium alloy used mainly for medical implant applications. It is an extra low interstitial alloy with a high purity, which confers improved ductility and fracture toughness. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2005) 54 (5): SS-930.
Published: 01 May 2005
... Sandvik SANMAC 4571 is a Sandvik hollow bar material. It is a stabilized austenitic stainless steel grade in hollow bar that meets the chemical requirements of DIN WNr. 1.4571 and UNS S31635, but has improved machinability. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1995) 44 (11): SS-622.
Published: 01 November 1995
... Sandvik 8R30 is an austenitic, titanium-stabilized stainless chromium-nickel steel. It is suitable for wet-corrosive service, but also has good mechanical strength at high temperatures. For applications requiring enhanced creep strength, it is recommended that the variant Sandvik 8R30H be used...
Journal Articles
Alloy Digest (1996) 45 (4): SS-643.
Published: 01 April 1996
... (20100P). In order to have the best ductility this grade should be used above 7OO C (1290°F). Sandvik can also deliver a modified version of Sanicro 31HT for use in the temperature range between about 550 and 700°C (1020 and 1290°F). The analysis and heat treatment of this version have been adapted...
Journal Articles
Alloy Digest (2006) 55 (3): SS-956.
Published: 01 March 2006
... that is both formable in the received condition and strong in the aged temper. Sandvik and Nanoflex are trademarks owned by Sandvik AB. Thermal expansion 30 100 °C 86 200 °F 30 200 °C 86 400 °F 30 300 °C 86 600 °F 30 400 °C 86 700 °F Grade 10-6/K 10-6/°F 10-6/K 10-6/°F 10-6/K 10-6/°F 10-6/K 10-6/°F...
Journal Articles
Alloy Digest (1995) 44 (1): Ni-475.
Published: 01 January 1995
... production. SANICRO and SANDVIK are trademarks of Sandvik AB. Sandviken, Sweden. Chemical composition (nominal), wt. %: Carbon 0.030 max. Silicon 0.5 max. Manganese 0.8 Chromium 21.5 Nickel 40.0 Molybdenum 3.0 copper 1.7 Titanium 0.8 Physical Properties: Density Specific heat capacity, mean value Temperature...
Journal Articles
Alloy Digest (2017) 66 (11): Ni-739.
Published: 01 November 2017
... Sandvik Sanicro 72HP is a corrosion- and oxidation-resistant grade (CRA) available as wire, particularly weld wire. Sanicro 72HP is commonly used as weld wire for joining NiCrFe alloys. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1984) 33 (3): SS-442.
Published: 01 March 1984
... SANDVIK Sanicro 28 is an all-purpose low-carbon stainless steel alloy for service in highly corrosive environments. It has exceptionally high resistance to various types of corrosive attack and has good weldability. Among its numerous applications are evaporator tubes in the production...
Journal Articles
Alloy Digest (1996) 45 (3): Ni-505.
Published: 01 March 1996
... environments. Sandvik and Sanicro are tmdemarks of Sandvik AB Chemical Composition, wt (Nod) :iEz Manganese ;!geym Molybdenum Copper Titanium 0.030 max. 0.5 max. F5 40:o 3.0 1.7 0.8 Physical Properties: wry, &cm3 own3 8.1 (0.30) S~cHearCapaciry,MeanValueat50-100 C(l20-210 F) J/kg. C (Btu/lb . F) 450 (0.105...
Journal Articles
Alloy Digest (2005) 54 (11): SA-552.
Published: 01 November 2005
...; PR is a Coromant insert geometry. Fig. 2 External medium machining recommendations for Ovako 280 hol- low bar using Sandvik Coromant P-Line inserts; ap = cutting depth, mm; fn = feed, mm/rev; vc = cutting speed, m/min; 4015 and 4025 are Coromant grades; PM is a Coromant insert geometry. ...
Journal Articles
Alloy Digest (1992) 41 (6): SS-530.
Published: 01 June 1992
... SANDVIK SANICRO 31HT is an austenitic iron-nickel-chromium alloy characterized by very good resistance to oxidation with good mechanical properties at elevated temperatures. It is recommended for resistance element sheathing, pyrometer tubes, airheaters, equipment for heat treating, furnace tubes...
Journal Articles
Alloy Digest (2013) 62 (1): SS-1133.
Published: 01 January 2013
... as Table UHA 23 and Code Case 1883 ASTM A182 Grade F61 UNS S32550 Forged Flanges NACE MR 01-75 General Characteristics: Ferralium 255 SD50 sets a new benchmark for superduplex as the first to state 570 MPa (83 ksi) as the minimum 0.2% proof stress. It offers excellent corrosion resistance in a wide variety...
Journal Articles
Alloy Digest (2008) 57 (2): SS-1007.
Published: 01 February 2008
... Ferralium 255-3AF is a modification of Ferralium 255 (see Alloy Digest SS-481, January 1987), one of the early superduplex stainless steels. The 255 alloy has been modified over time with special chemistry, heat treatment, and production methods. This version is the age-hardened grade...
Journal Articles
Alloy Digest (2007) 56 (1): SS-983.
Published: 01 January 2007
... in the reduction of mechanical properties due to stress relief of the work-hardened microstructure. Corrosion Resistance: The excellent corrosion resistance of this grade is shown in Table 2 compared to other grades. Table 1 Machining Advice Cutting speed Feed rate Depth of cut Operation m/min ft/min rpm mm/rev...