Alloy Digest (2010) 59 (8): SS-1074.
Published: 01 August 2010
... Sandvik T302 HS is a general purpose austenitic stainless steel with respect to corrosion resistance only in a spring temper for higher strength. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength It also includes...