Alloy Digest (2017) 66 (11): Ni-739.
Published: 01 November 2017
... Sandvik Sanicro 72HP is a corrosion- and oxidation-resistant grade (CRA) available as wire, particularly weld wire. Sanicro 72HP is commonly used as weld wire for joining NiCrFe alloys. This datasheet provides information on composition, physical properties, hardness, and tensile properties...