Alloy Digest (1994) 43 (10): Ni-467.
Published: 01 October 1994
... Sandvik SANICRO 69 is an austenitic nickel-chromium-iron alloy with increased chromium composition for enhanced resistance to pressurized water in nuclear systems. Its primary application is steam generators in PWR’s. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1992) 41 (6): SS-530.
Published: 01 June 1992
... SANDVIK SANICRO 31HT is an austenitic iron-nickel-chromium alloy characterized by very good resistance to oxidation with good mechanical properties at elevated temperatures. It is recommended for resistance element sheathing, pyrometer tubes, airheaters, equipment for heat treating, furnace tubes...
Journal Articles
Alloy Digest (1995) 44 (11): SS-622.
Published: 01 November 1995
... or 19.9.LR are recom- mended. For application at temperatures above 4OO C (750°F). wire elec- nodeshods Sandvik-Sanicro 72 should be used in gas-shielded arc welding and covered electrodes Sanicro 72 in manual metal- arc welding. (Sanicro is a trademark of Sandvik AB) Corrosion Resistance: General...