Alloy Digest (2017) 66 (10): Ni-737.
Published: 01 October 2017
... Sandvik Sanicro 59 is a corrosion resistant grade (CRA) available as wire, particularly weld wire. Sanicro 59 is used to weld most of the nickel alloys such as alloy 59, C-22, C-276, etc. It can also be used for joining nickel alloys with duplex stainless steels, super duplex stainless steels...
Journal Articles
Alloy Digest (2018) 67 (9): SS-1293.
Published: 01 September 2018
...) 210 (30.5) 520 (75) 600 (1112) 180 (26) 205 (30) 500 (72.5) 650 (1202) 180 (26) 210 (30.5) 480 (70) 700 (1292) 180 (26) 195 (28) 455 (66) 750 (1382) 180 (26) 195 (28) 410 (59) 800 (1472) 180 (26) 195 (28) 355 (51.5) Table 2 Creep properties of Sandvik Sanicro 25 Temperature, °C (°F) Creep properties...
Journal Articles
Alloy Digest (2001) 50 (8): Ni-572.
Published: 01 August 2001
... Sandvik Sanicro 63 was developed specifically for use as outer cladding of composite tubes in service as superheater materials for waste-derived fuel plants. It is a modification of UNS N06625. Typical inner components of the composite tubes are Sandvik 4L7 and Sandvik HT8. This datasheet provides...
Journal Articles
Alloy Digest (1992) 41 (4): SS-526.
Published: 01 April 1992
... is also excellent. *Sandvik, SAF 2507 and Sanicro are trademarks of Sandvik AEL Chemical Composltion (Nominal): Carbon 0.03 max. Silicon 0.8 max. Manganese 1.2 max. Phosphorus 0.035 max. SU1ft.U 0.02 max. Chromium 25 Nickel 7 Molybdenum 4 Nitrogen 0.3 Iron Remainder. Temperature. C (OFI 30 (85) Physical...
Journal Articles
Alloy Digest (1989) 38 (8): SS-267.
Published: 01 August 1989
... are recommended for TIG and MIG welding in cases where there is a risk of weld metal stress cracking. For manual metal-arc welding. use Sandvik 29.9R. 25.20R or Sanicro 72. Corrosion Resistance: Sandvik 4C54 is resistant to oxidation at constant and cyclical varying temperatures. The limiting service temperature...
Journal Articles
Alloy Digest (2004) 53 (7): Ni-622.
Published: 01 July 2004
... of Sandvik AB. Table 1 Typical Room-Temperature Tensile Properties Yield strength, Thickness Tensile strength 0.2% offset Elongation in mm in. MPa ksi MPa ksi 2 in., % 3.175 0.125 744 108 348 50.5 59 6.35 0.250 703 102 344 49.9 66 12.7 0.500 689 100 318 46.1 72 25.4 1.000 710 103 319 46.3 66 63.5 2.5000 689...
Journal Articles
Alloy Digest (1997) 46 (11): SS-699.
Published: 01 November 1997
...- mends wire electrodes and rods Sandvik 72. In manual metal-arc welding covered ekcmdes Sandvik Sanicro 72 are recom- mended. For application at temperatures up to 400 C (750 m. welding wire/d Sandvik 19.9.NbSi. 19.9.Nb. 19.9.LSi or 19.9.L and covered electmdes Sandvik 19.9.NbR or 19.9LR are recommended...
Journal Articles
Alloy Digest (2002) 51 (5): SS-852.
Published: 01 May 2002
... applications, filler metals of the high-nickel type, for example Sanicro 72, can be used. Contact the producer for further rec- ommendations. Corrosion Resistance: Gas Corrosion. Sandvik 3R60HT can be used in air up to 850 °C (1560 °F), in steam up to 750 °C (1380 °F), and in ammonia synthesis gas up to about...
Journal Articles
Alloy Digest (2001) 50 (1): SS-812.
Published: 01 January 2001
... is somewhat impaired. For service in this temperature range, the producer recommends the use of Sandvik Sanicro 31HT (see Alloy Digest SS-643), which has better struc- tural stability. Maximum service temperature in air is 1100 °C (2010 °F). Product Forms Available: Seamless tube and pipe are generally...