Alloy Digest (1997) 46 (2): SS-671.
Published: 01 February 1997
... Sandvik Safurex is a high alloy duplex (austenitic-ferritic) stainless steel primarily developed to withstand the corrosive environments present in the urea industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...