Alloy Digest (2007) 56 (10): SS-999.
Published: 01 October 2007
... Sandvik SAF 2707 HD is a duplex stainless steel, highly alloyed at 27 Cr, 6.5 Mo, 4.8 Mo, 1.0 Co, and 0.4 N. The alloy can be used in aggressive acidic chloride conditions. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...