1-20 of 44 Search Results for

Sandvik High-N

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2019) 68 (8): SS-1308.
Published: 01 August 2019
... Sandvik High-N is both N and Mo alloyed austenitic stainless steel. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion and wear resistance as well as forming and heat treating. Filing Code: SS-1308...
Journal Articles
Alloy Digest (2000) 49 (6): SS-793.
Published: 01 June 2000
... Sandvik Bioline High N is a molybdenum-alloyed stainless steel for implant applications. Corrosion resistance to physiological environments is good. The alloy is of high purity and has an excellent surface finish. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2007) 56 (10): SS-999.
Published: 01 October 2007
... Sandvik SAF 2707 HD is a duplex stainless steel, highly alloyed at 27 Cr, 6.5 Mo, 4.8 Mo, 1.0 Co, and 0.4 N. The alloy can be used in aggressive acidic chloride conditions. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2000) 49 (5): SS-784.
Published: 01 May 2000
... implantable medical devices. Producer: Sandvik Steel Company Tubular Products Division Scranton, PA 18501-1220 (570) 585-7511 (570) 585-7513 (fax) In Sweden: Sandvik Steel Sandviken +46 26-26 30 00 +46 26-25 17 10 (fax) ISSN: 002-614X SS-784B Temperature °F °C 210 100 175 80 140 60 105 40 7 20 316LVM High-N...
Journal Articles
Alloy Digest (2014) 63 (5): SS-1172.
Published: 01 May 2014
... Environments. This alloy has been developed to resist high temperatures in chloride environments. Owing to its high content of Cr, Mo, and N, the alloy has a very high PRE number, > 50, which ensures resistance against pitting. See Fig. 1 for critical pitting temperatures. Sour Environments. This alloy has...
Journal Articles
Alloy Digest (1994) 43 (10): Ni-467.
Published: 01 October 1994
..., hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-467. Producer or source: Sandvik. Producer or Source: Sandvik Copyright © ASM International® 1996 1996...
Journal Articles
Alloy Digest (1995) 44 (7): Ni-483.
Published: 01 July 1995
... SANDVIK SANICRO 70 is an austenitic alloy with good high temperature resistance to carburization and nitridation. The alloy is also very resistant to chloride-ion stress-corrosion cracking and to hydrogen chloride. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1997) 46 (10): Ti-110.
Published: 01 October 1997
... as fracture toughness. It also includes information on high temperature performance, and corrosion resistance. Filing Code: TI-110. Producer or source: Sandvik. Producer or Source: Sandvik Copyright © ASM International® 1997 1997 ASM International chemical composition corrosion-resistant alloys...
Journal Articles
Alloy Digest (1995) 44 (11): SS-622.
Published: 01 November 1995
... Sandvik 8R30 is an austenitic, titanium-stabilized stainless chromium-nickel steel. It is suitable for wet-corrosive service, but also has good mechanical strength at high temperatures. For applications requiring enhanced creep strength, it is recommended that the variant Sandvik 8R30H be used...
Journal Articles
Alloy Digest (1987) 36 (7): SS-487.
Published: 01 July 1987
... SANDVIK SAF 2205 is an extra-low carbon, ferritic-austenitic stainless steel. It has high resistance to stress-corrosion cracking; pitting; service and general corrosion. It has roughly twice the yield strength of austenitic stainless grades and it has good weldability. This datasheet provides...
Journal Articles
Alloy Digest (2015) 64 (5): SS-1209.
Published: 01 May 2015
... Sandvik SAF 3207 HD is a hyper-duplex stainless steel with high strength and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information...
Journal Articles
Alloy Digest (1997) 46 (9): Ti-109.
Published: 01 September 1997
... Sandvik Ti-3Al-2.5V Grade 9 titanium-aluminum alloy offers excellent corrosion resistance, especially to chloride media, and has a high strength-to-weight ratio, which is especially suitable for use in aerospace applications. Tubing can be produced having a CSR (contractile strain ratio...
Journal Articles
Alloy Digest (1966) 15 (2): SS-177.
Published: 01 February 1966
... SANDVIK 11R51 is a stainless steel having high fatigue and tensile strengths. It is recommended for springs requiring corrosion resistance and high torque values. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2015) 64 (2): SS-1203.
Published: 01 February 2015
... steels to pitting is the PRE number (Pitting Resistance Equivalent). The PRE is defined as, in weight %: PRE = %Cr + 3.3 × %Mo +16 × %N. Sandvik SAF 2205 PM has a chemical composition within UNS S32205, which is optimized within the UNS S31803 range in order to provide a high PRE value, greater than 35...
Journal Articles
Alloy Digest (1994) 43 (11): SS-575.
Published: 01 November 1994
... SANDVIK 3R69 is a nitrogen-alloyed, high-strength variant of AISI 316L, used predominantly in the urea industry. The steel has guaranteed maximum ferrite content of 0.6%. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2001) 50 (9): SS-831.
Published: 01 September 2001
... joinability physical properties SANDVIK SANICRO 28 tensile properties waste-derived fuel plants workability thermal properties UNS N08028 Sandvik Sanicro 28 composite tube is used in services as superheater material for waste-derived fuel plants. SANDVIK® SANICRO® 28 (Composite Tube High-Temperature...
Journal Articles
Alloy Digest (1995) 44 (5): SS-593.
Published: 01 May 1995
... Sandvik 3R60 is an austenitic stainless steel, a highly purity variant of AISI Type 316L for the urea industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high...
Journal Articles
Alloy Digest (2015) 64 (1): SS-1195.
Published: 01 January 2015
... Sandvik Pressurfect is an austenitic chromium-nickel stainless steel with low carbon content used for high-pressure gasoline direct injection (GDI) fuel system. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength...
Journal Articles
Alloy Digest (1995) 44 (10): SS-614.
Published: 01 October 1995
... are recommended. Machinability: Sandvik SANMAC 316L has very good machining properties. (Detailed recommendations for the choice of tools and cutting data are available from the producer.) Besides sulfides, SANMAC 316L contains oxide inclusions that promote chipbreaking and have a lubricating effect at high...
Journal Articles
Alloy Digest (1989) 38 (4): SS-504.
Published: 01 April 1989
..., and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-504. Producer or source: Sandvik. Producer or Source: Sandvik Copyright © ASM...