Alloy Digest (2011) 60 (9): SS-1102.
Published: 01 September 2011
... Sandvik Bioline 7C27 an alloy that hardens well and has good corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming and heat treating. Filing Code: SS-1102. Producer or source...