Alloy Digest (2005) 54 (11): SS-946.
Published: 01 November 2005
... Sandvik Bioline 4C27A is a hardenable 13% Cr stainless steel used in precision instruments. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: SS-946. Producer...